Grade |
ISO Code |
Density
g/cm3 |
Hardness
HRA |
T.R.S
MPa |
Applications recommended |
YG3 |
K05 |
15.10 |
92.0 |
1400 |
Suitable for finishing of cast iron and nonferrous metal. |
YG6X |
K10 |
14.95 |
91.5 |
1800 |
The finishing & semi-finishing of cast iron and nonferrous metals and also for the machining of manganese steel and hardening steel. |
YG6 |
K15 |
14.95 |
90.5 |
1900 |
Suitable for the roughing of cast iron and light alloys and also for the milling of cast iron and low-alloy steel. |
YG8 |
K20 |
14.80 |
89.5 |
2200 |
YW1 |
M10 |
13.10 |
91.6 |
1600 |
Suitable for finishing and semi-finishing of stainless steel and conventional alloy steel. |
YW2 |
M20 |
13.00 |
90.6 |
1800 |
The grade can be used for the semi-finishing of stainless steel and low-alloy steel and it is mainly used for the machining of railway wheel hubs. |
YT15 |
P10 |
11.4 |
91.5 |
1600 |
Suitable for the finishing and semi-finishing for steel and cast steel with a moderate feed rate and rather high cutting speed. |
YT14 |
P20 |
11.6 |
90.8 |
1700 |
Suitable for the finishing and semi-finishing of steel and cast steel. |
YT5 |
P30 |
12.9 |
90.5 |
2200 |
Suitable for the heavy duty rough turning of and cast steel with a big feed rate at a medium and low speed under unfavorable working conditions. |